Aircraft Structures Nickel Based Superalloys Precipitation Hardened GH4145 800°C

  • 1
  • 2

Brand Name : XUNSHI

Model Number : GH4145

Certification : ISO9001

Place of Origin : China

MOQ : 50kg

Price : Negotiable

Payment Terms : T/T

Supply Ability : 1000k per week

Delivery Time : 30-35 days

Packaging Details : Plywood case

Equal grades : Inconel X-750, NiCr15Fe7TiAl, 2.4669,UNS N07750

Melting range : 1395°C~1425°C

Density : 8.25g/cm3

Forms of supply : Plate, strip, bar, forging, ring, wire, tube

Spec : GB/T 14992

Product Name : Nickel Cobalt Alloy

Contact Now

GH4145 Nickel Alloy Precipitation-hardened Superalloy up to 800°C Application


GH4145 is a precipitation-hardenable nickel-chromium alloy used for its corrosion and oxidation resistance and high strength at temperatures up to 1300°F. Although much of the effect of precipitation hardening is lost with increasing temperature over 1300°F, heat-treated material has useful strength up to 1800°F. GH4145 also has excellent properties down to cryogenic termperatures.

Depending on the application and the properties desired, various heat treatments are employed. For service above 1100°F, particularly where loads are to be sustained for long times, optimum properties are achieved by solution treating (2100°F) plus stabilization treating (1550°F) plus precipitation treating (1300°F). For service below 1100°F, the alloy may be strengthened by precipitation treating after hot or cold working or by precipitation treating after equalizing or solution treating. A furnace-cooling treatment is also used to develop optimum properties for some applications.


Chemical compositin

ElementCCrNiCoAlTiFeNbMnSiSPCu
Weight(%)0.08 max14.00~17.0070.00 min1.00 max0.40~1.002.25~2.755.00~9.000.70~1.201.00 max0.50 max0.010 max0.015 max0.50 max

Features

  • Good creep rupture strength at high temperatures
  • Not as strong as Nimonic 90
  • Very good at cryogenic temperatures
  • Age hardenable
  • High temperature dynamic applications

Applications

  • Nuclear reactors
  • Gas turbines
  • Rocket engines
  • Pressure vessels
  • Aircraft structures

Available Product Forms
Sheet, strip, plate, round bar, flat bar, forging stock, hexagon, wire, tube and extruded


Product Tags:

nickel based alloys

      

high temperature nickel alloys

      
Quality Aircraft Structures Nickel Based Superalloys Precipitation Hardened GH4145 800°C for sale

Aircraft Structures Nickel Based Superalloys Precipitation Hardened GH4145 800°C Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Suzhou Xunshi New Material Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)